Improvement of flotation circuit performance of Sungun copper complex (plant of phase 1)

Document Type : research - paper

Authors

1 Tarbiat Modares University

2 Mining Engineering Department, Tarbiat Modares University, Tehran, Iran

3 Mineral Processing Plant, Sungun Mine, Tabriz, Iran

Abstract

In this study, the feasibility of improving the flotation circuit performance of a phase 1 of Sungun copper plant was investigated. For this purpose, circuit performance was first monitored ., It was found that in the rougher stage the some copper exists in fractions greater than 106 and smaller than 38 microns was lost. Final concentrate analysis taken on different days showed that the copper grade decreased due to the iron content increasing. Mineralogical studies also confirmed the maximum presence of pyrite in the final concentrate. Field surveys of the flotation circuit showed that there are many technical problem in the circuit that affect on the flotation process. These drawbacks including the presence of thick tubes at the surface of the re-cleaner cell, the lack of a standard pattern of wash water distribution and jet spraying. Measurement of pH in different points of the circuit showed a decrease of pH below 11 and so hydrophobicity of pyrite caused. Measurement of operating variables in the circuit showed that the wash water rate and gas rate used in the circuit were higher and lower than the values suggested by the researchers and the designer, respectively. Due to the deficiencies identified in the performance evaluation phase, laboratory tests were designed and performed in two stages using mechanical flotation cell and column flotation cell. Adjusting the gas rate and the wash water rate at the laboratory scale at the intervals suggested by the researchers resulted in the increase in 3% grade and 10% recovery.

Keywords


منابع

[1] سلحشور, عباس. بهرامی, عطااله و عبدالهی شریف, جعفر.1397، «طراحی بهره برداری معادن روباز با نگرش کاهش اثرات زیست محیطی در معدن مس سونگون». مهندسی منابع معدنی، دوره سوم، شماره 3، 43 تا 55.
[2] صبوری, حسین. 1393. «بهینه سازی عیار و بازیابی مولیبدن در مدار فلوتاسیون مس- مولیبدن مطالعه موردی مجتمع مس سونگون», دانشکده معدن، نفت و ژئوفیزیک, دانشگاه صنعتی شاهرود.
[3] باقریان, اصغر, 1385، «فرآیند پر عیار سازی مس در کارخانه تغلیظ مس سونگون», شرکت ملی صنایع مس ایران، مجتمع مس سونگون.
[4] Laurila, H., J. Karesvuori, and O. Tiili, 2002, “Strategies for instrumentation and control of flotation circuits. Mineral Processing Plant Design” Practice and Control, 2002. 2: p. 2174-2195.
[5] Yianatos, J. and A. Levy.1989. “Estimation of gas holdup, diameter and apparent density ofmineralized bubbles in industrial flotation columns”. in Intern. Colloquium Developments in Froth Flotation. SAIMM Western Cape Branch, South Africa.
[6] Yianatos, J.B. and L.G. Bergh, 1995 “Troubleshooting industrial flotation columns”. Minerals Engineering,. 8(12): p. 1593-1605.
[7] Banisi, S. and J.A. Finch, 2001 “Testing a flotation column at the Sarcheshmeh copper mine”. Minerals Engineering, 14(7): p. 785-789.
[8] رضایی راد، محمد, 1388، تحلیل مدار فلوتاسیون پر عیار کنی نهایی مجتمع مس میدوک, در دانشکده فنی و مهندسی گروه مهندسی معدن, دانشگاه شهید باهنر کرمان.
[9] جلیلی­نیا، فریبا, 1391، امکان سنجی کاهش پیریت (سولفور) در کنسانتره سولفیدی مدار فلوتاسیون مجتمع مس سرچشمه, در دانشکده فنی و مهندسی بخش مهندسی معدن, دانشگاه شهید باهنر کرمان.
[10] قربانی، کریم, 1391، بررسی تأثیر درجه آزادی، نوع و بافت کانی های حاوی مس در عملیات فلوتاسیون کارخانه تغلیظ مس سونگون, در دانشکده فنی و مهندسی، گروه مهندسی معدن, دانشگاه بین المللی امام خمینی قزوین.
[11] لطفی، علی, 1392، رفتار سنجی کانی های موجود در مدار فرآوری مجتمع مس سونگون و تأثیر آن بر راندمان کلی و ارائه مدل پیش بینی عملکرد, در دانشکده مهندسی معدن، نفت و ژئوفیزیک, دانشگاه صنعتی شاهرود.
[12] فرامرزی، حمید, 1394، امکان سنجی بازداشت پیریت از کنسانتره مدار فلوتاسیون کارخانه مجتمع مس سونگون, در دانشکده فنی و مهندسی، گروه مهندسی معدن, دانشگاه بین المللی امام خمینی (ره) قزوین.
[13] بهجت جباری، مجید. محمودی میمند، محمد, 1396، بررسی علل افت بازیابی و عیار مس کنسانتره نهایی کارخانه تغلیظ مجتمع مس سونگون و ارائه راهکارهای عملی برای حل مشکل, امور تحقیق و توسعه تحقیقات فرآوری مواد: شرکت ملی صنایع مس ایران- مجتمع مس سرچشمه.
[14] بنیسی، صمد. یار احمدی، محمدرضا, 1391، موازنه جرم در سیستم های فرآوری مواد, ویرایش دوم, هرمزگان: دانشگاه هرمزگان.
[15] Hodouin, D., et al., 1998 “Reconciliation of mineral processing data containing correlatedmeasurement errors”. International Journal of Mineral Processing, 54(3): p. 201-215.
[16] Hodouin, D., T. Gelpe, and M. Everell, 1982 “Sensitivity analysis of material balance calculations—An application to a cement clinker grinding process”. Powder Technology, 32(1): p. 139-153.
[17] Bulatovic S. M. 2007, Handbook of flotation reagents: chemistry, theory and practice: Volume 2: flotation of sulfide ores. Elsevier.